ChatDiagram
ceramic target · sintering cracking · fishbone diagram

Key Factor Analysis of Cracking in Ceramic Target Sintering Process

유형 피시본 다이어그램표준 Ishikawa (1968) cause-and-effect엔진 schematex-fishbone업데이트됨 2026. 8. 27.
Key Factor Analysis of Cracking in Ceramic Target Sintering Process
Drawing preview
상황

A ceramic sputtering target manufacturer observes cracking during sintering, reducing yield. This fishbone structures potential causes across the 6M categories to prioritize investigation.

이 도면에 담긴 내용

그 이면의 의사결정을 읽어 보세요.

01

Use 6M categories with alternating top/bottom ribs to keep layout readable.

02

Assign side and order to each category to prevent automatic alternating overlap.

03

Include sub-causes only where a primary cause has specific contributing factors.

Use this template when analyzing root causes of defects in ceramic target forming or similar powder sintering processes; adapt categories and causes to specific material systems.